Pass Your Red Seal

Bricklayer Flashcard Match

Online Red Seal Exam Preparation, built on official standards
Flashcard Match10 pairs · 1 decoyChecked at the endStart matching

Set up a round

Cards from

Pairs per round

Blocks

Decoys

250 cards to draw from

ACommon occupational skills28
BGeneral masonry practices48
CBuilds masonry systems54
DBuilds natural stone systems26
EBuilds chimneys and fireplaces26
FInstalls refractories and corrosion resistant materials20
GRestoration28
HAdditional masonry20

Your rounds

Kept on this device
Average79%
Best100%

Checking

What a checked pair looks like
Browse the 20 free cards and explanations

A mason's spirit level may have been knocked out of true. With no second level and no surface known to be level, how is its level vial checked for accuracy?

Answer: Read the bubble on a flat, nearly level surface, then turn the level end for end on the same spot; a true vial reads the same both ways.

Reversing the level separates the two errors: a tilt in the surface shows the same way in both positions, while an error in the vial reverses and appears as a difference between the readings. Plumb vials are checked by the same reversal against a vertical surface. A level that fails is adjusted to the maker's instructions or replaced.

Exam trap: Set it on a surface that looks level and check that the bubble centres: without reversing it, a tilt in the surface cannot be told apart from an error in the vial.

Standard reference: RSOS 2021 A-2.01.02L

For excavation beside an existing masonry building, what category of buried services may remain unmarked after public-utility locates are complete?

Answer: Privately owned services, such as feeds to outbuildings; these also require locating before excavation.

A locate covers the services within its scope, not every line on a property. Private feeds may be outside the public utility’s ownership. The excavation plan must account for all buried services through the appropriate owners or locating services.

Exam trap: Treating completed public-utility locates as proof that the entire excavation area is free of other services leaves private feeds unaccounted for.

Standard reference: RSOS 2021 A-4.02.01L

Two foundation walls will get the same cement parge: one of new, open-textured concrete block, the other of clean, smooth, dense poured concrete. Which wall needs a bonding agent before it is parged, and why?

Answer: The poured concrete wall: its dense, smooth face gives the parge too little suction and texture to grip, while dampened open-textured block bonds without one.

Parge bonds by suction, which draws cement paste into the substrate's pores, and by keying into its texture. Dampened open-textured block supplies both. A dense, smooth concrete face supplies little of either, so a bonding agent suited to the exposure is applied first (or the face is mechanically roughened), and the parge is timed to the agent as its maker directs.

Exam trap: The block wall, because it is the more porous: that porosity is what gives dampened block its suction and key; the dense concrete face is the one the parge cannot grip.

Standard reference: RSOS 2021 B-6.02.02P

Which brick bond lays a header and a stretcher alternately along every course, with each header centred over the stretcher below?

Answer: Flemish bond.

Flemish bond alternates headers and stretchers within each course, each header centred on the stretcher beneath, which gives a quarter-unit lap. At corners a closer (queen closer) is cut next to the corner header to set that lap. In solid walls the headers also bond the two wythes together.

Exam trap: English bond: it alternates whole courses of headers with whole courses of stretchers, rather than mixing the two within one course.

Standard reference: RSOS 2021 B-7.01.01L

A proprietary acid-based masonry cleaner's label calls for 1 part concentrate to 6 parts water. A crew needs 14 L of mixed solution. How much concentrate and how much water are used?

Answer: 2 L of concentrate and 12 L of water.

1 + 6 = 7 parts in total; 14 L ÷ 7 = 2 L per part. Concentrate = 1 × 2 = 2 L; water = 6 × 2 = 12 L; check 2 + 12 = 14 L. Measure the water into a plastic pail first, then add the concentrate to it, as with any acid-based cleaner.

Exam trap: 2.33 L of concentrate, from 14 ÷ 6: that treats '1 to 6' as one-sixth of the total, but the ratio means 7 parts, so this mix is too strong.

Standard reference: RSOS 2021 B-7.03.03P

Which property of hardened mortar is regarded as the most important to a masonry wall's strength and its resistance to water penetration?

Answer: Bond: both the extent of contact and the strength of adhesion between the mortar and the masonry units.

Most leaks and cracks in masonry occur at the mortar-unit interface, not through the mortar itself. Extent of bond depends on workable, water-retentive mortar, units of suitable suction, full joints and good tooling; bond strength resists cracking under movement and wind. A modest-strength mortar with good bond outperforms a high-strength one with poor bond.

Exam trap: Compressive strength: it is easy to specify and test, but a strong mortar with poor bond still cracks and leaks at the joint faces.

Standard reference: RSOS 2021 B-8.02.01L

Why are the ends of a lead normally racked back course by course rather than toothed with alternate units projecting?

Answer: A racked end lets the infill be laid with full, well-packed head and bed joints; toothing pockets are hard to fill and leave voids.

When the wall between leads is filled in, each closing unit must be bedded and buttered so its joints fill solid. A racked end is open on top, so units go in the normal way. A toothed pocket must be filled from the side, so its joints are often left partly empty, weakening the wall and letting water in. Toothing is used only where the specification allows it.

Exam trap: That racking makes the lead easier to plumb and level: the lead is plumbed the same either way; racking is about solid joints where the infill meets the lead.

Standard reference: RSOS 2021 C-9.01.04P

A 2 200 mm wide opening in a load-bearing block wall needs a precast concrete lintel with at least 200 mm of bearing at each end. Lintels are stocked only in lengths that are whole multiples of 400 mm. Which length is used, and how is it placed?

Answer: 2 800 mm, centred over the opening: the minimum is 2 600 mm, and 2 800 mm gives 300 mm of bearing at each end.

Minimum length = opening + bearing at both ends: 2 200 + 2 × 200 = 2 600 mm. The nearest stocked multiples of 400 mm are 2 400 and 2 800 mm; 2 400 is too short, so 2 800 mm is used. Centred, it bears (2 800 − 2 200) ÷ 2 = 300 mm at each end; the extra bearing spreads the end reactions over more masonry.

Exam trap: 2 400 mm, adding the 200 mm bearing only once: centred, that leaves 100 mm at each end, half the required bearing.

Standard reference: RSOS 2021 C-9.02.10P

Sand-set concrete pavers have been laid and plate-compacted into their bedding sand, but the pile of joint sand is soaked from overnight rain. What is done with that sand before it goes into the joints?

Answer: Dry it first: spread it thin on a clean, hard surface until it runs freely, then sweep it in and compact until the joints are full.

Joint sand locks the pavers together only when it fills each 2–5 mm joint to the bottom. Wet sand clumps and bridges near the top of the joint, leaving voids below that the plate compactor cannot shake down. Dry sand flows into the joints as the compactor vibrates it; two or three passes with topping up fill them, and the excess is swept off.

Exam trap: Sweeping the wet sand in and counting on rain or a hose to wash it down: it bridges near the top, washes out and leaves partly empty joints with little interlock.

Standard reference: RSOS 2021 C-10.02.04P

A painted concrete foundation wall is to receive adhered stone veneer. Water sprinkled on it beads up, and the paint must stay in place. How must the wall be prepared?

Answer: Mechanically fasten corrosion-resistant metal lath to the concrete and apply a full scratch coat over it before setting the stone.

Mortar bonds only to a clean, rough, absorptive surface, and beading shows the paint has sealed the concrete. Mortar on paint is only as strong as the paint's grip on the wall. When the coating cannot be removed, lath fixed into the concrete with concrete screws or powder-actuated fasteners carries the scratch coat independently of the paint.

Exam trap: Brushing a bonding agent over the paint and setting stone directly: the veneer then hangs on the old paint film, which can peel off under the load.

Standard reference: RSOS 2021 C-12.01.02L

A one-piece cut-stone lug sill spans a window opening with its ends built into the masonry piers on each side, and several more courses are still to be laid on the piers. How is the sill bedded when it is set?

Answer: On mortar under its two ends (the lugs) only; the joint under the middle is left open, then filled and pointed after the wall is complete.

The piers settle slightly as masonry is added above them, but the unloaded middle of the sill does not. A full bed makes the middle a rigid support, so the sill bends over it and cracks. Bedding only the lugs lets the sill settle with the piers; the open joint under the middle is cleaned, filled and pointed once the masonry above is complete.

Exam trap: A full mortar bed along its whole length; as the loaded piers settle, the sill bridges on the stiff middle bed and cracks.

Standard reference: RSOS 2021 D-13.02.02P

Why can a torch be used to give granite a rough thermal (flamed) finish, while marble and limestone cannot be finished that way?

Answer: Granite's quartz and feldspar crystals expand unevenly in the flame and pop off, leaving a rough crystalline face; calcite stones scorch instead.

Flaming depends on rapid, uneven expansion of hard, mixed minerals and trapped moisture: the surface crystals rupture and flake away. Marble and limestone are calcite, which does not spall that way; the heat discolours and breaks down the surface. Flaming removes a few millimetres and lowers strength, so flamed panels are cut thick enough to allow for it.

Exam trap: That granite is just harder and more heat-resistant; flaming works because the heat bursts its quartz and feldspar crystals off the face, not because granite withstands it.

Standard reference: RSOS 2021 D-14.02.03P

A chimney's upslope face meets a 6-in-12 roof 4.0 m (measured horizontally) below the ridge. Under the National Building Code (NBC), how far must the flue extend above that highest point of roof contact?

Answer: At least 2.1 m (about 7 ft) above the highest point where the chimney meets the roof.

The flue must be at least 900 mm above the highest roof contact and 600 mm above any roof surface or structure within 3 m horizontally (NBC 9.21.4.4). The ridge is beyond 3 m, but the roof itself 3 m upslope is 3 m × 6/12 = 1.5 m higher than the contact point: 1.5 m + 0.6 m = 2.1 m, which governs over 0.9 m.

Exam trap: 0.9 m because the ridge is more than 3 m away: the sloping roof within 3 m upslope is still a roof surface, and it rises 1.5 m above the contact point.

Standard reference: RSOS 2021 E-15.02.03P

Before the smoke chamber is built, a new cast-iron damper is placed on the top course of firebrick. What material separates the damper from that firebrick, and how is the damper set on it?

Answer: A strip of noncombustible, compressible material such as mineral wool; the damper is levelled and sealed on it but not mortared or bonded to the firebox.

Cast iron expands more than the surrounding masonry as it heats. A noncombustible, compressible layer between the damper and the top of the firebox, with the damper only levelled and sealed and not bonded, lets the frame grow and shrink without cracking the firebrick, the breast brickwork or the smoke shelf.

Exam trap: Bedding the damper solid in refractory mortar: the mortar survives the heat, but it locks the frame in place, so the frame's expansion cracks the firebox and facing.

Standard reference: RSOS 2021 E-16.03.02P

What rule governs which refractory mortar is used to lay a given refractory brick, such as silica, high-alumina or fireclay brick?

Answer: Match the mortar's composition and temperature rating to the brick: silica mortar for silica brick, high-alumina for high-alumina, fireclay for fireclay.

A mortar of different chemistry can react with the brick at service temperature, fluxing and melting at the joint, or expand and shrink differently and open up. The maker pairs each brick with a mortar of similar composition rated for the service temperature. The joint is already the weakest part of the lining, so it must not also be the odd material.

Exam trap: Using the most refractory high-alumina mortar for every brick; alumina acts as a flux on silica brick at high temperature, so compatibility, not the highest rating, governs.

Standard reference: RSOS 2021 F-17.02.03P

A chemical-resistant epoxy mortar is proportioned by weight at resin 2 : hardener 1 : filler 9. A partial batch is to be made with 1.6 kg of resin. How much hardener and filler are needed?

Answer: 0.8 kg of hardener and 7.2 kg of filler, giving 9.6 kg of mortar.

Proportions by weight scale from one part: 1.6 kg of resin ÷ 2 = 0.8 kg per part. Hardener = 1 × 0.8 = 0.8 kg; filler = 9 × 0.8 = 7.2 kg; total 1.6 + 0.8 + 7.2 = 9.6 kg. Partial kits are weighed on a scale, never judged by eye, and each batch is sized so it can be placed within the mortar's pot life.

Exam trap: 1.6 kg of hardener and 14.4 kg of filler, treating the 1.6 kg of resin as one part; the resin is two parts, so one part is 0.8 kg.

Standard reference: RSOS 2021 F-18.02.03P

A new length of galvanized steel through-wall flashing is lapped onto existing copper flashing in a cavity wall that stays damp. What happens at the lap?

Answer: Galvanic corrosion: the zinc coating, then the steel, corrodes rapidly where it touches or receives runoff from the copper, and the flashing fails.

When dissimilar metals are joined in the presence of moisture, the less noble metal becomes the anode and corrodes. Zinc and steel sit well below copper in the galvanic series, so they are consumed, and runoff carrying copper attacks zinc even without contact. New flashing is copper or another metal known to be compatible, as the job specifications require.

Exam trap: That the copper corrodes because it turns green: copper is the more noble metal, so it is the zinc and steel that are eaten away.

Standard reference: RSOS 2021 G-19.02.02P

Hard portland cement mortar must be cut out of a brick wall's 10 mm joints for repointing, and the specification lets a skilled mason use a diamond-blade grinder. On which joints may the grinder be used, and how is the rest of the mortar removed?

Answer: On the bed joints only, cutting along the middle of each; the head joints and the mortar left at the joint edges are cleared by hand with a chisel and hammer.

A long bed joint lets the blade follow the joint centre, but a short head joint ends at the brick above and below, so any slip or overrun cuts into the units and widens the joint. Hand tools clear the head joints and pare the remaining mortar off the sides of each cut, leaving square, clean joint edges and undamaged arrises.

Exam trap: Grinding the head joints too, carefully: a short vertical cut easily overruns into the brick above or below, overcutting and widening the joint.

Standard reference: RSOS 2021 G-20.02.01P

A 350 kg carved limestone cornice unit, finished on its face, soffit and ends, must be lowered into a gap between two units already set, leaving 10 mm joints. Slings could not be withdrawn once it landed. How should it be rigged for setting?

Answer: With a lewis (or lewis pins) set in a hole cut in the top bed over the unit's centre of gravity, so it lowers straight onto its bed.

A lewis grips the stone from inside a hole in its top bed, so nothing wraps the carved faces and nothing is trapped under or beside the unit when it lands. A hole over the centre of gravity lets the unit hang level, and the course above hides it. The hole is arranged with the fabricator; lewis pins are not used in thin stone (under about 90 mm).

Exam trap: A scissor clamp (stone grab): its jaws must grip the finished ends or carved face, would not fit or release in the 10 mm joints, and would mark the stone.

Standard reference: RSOS 2021 H-22.01.02L

An arch template is to be set over a window that is already installed in a brick-veneer opening. What should carry the template?

Answer: Its own posts on firm bearing (a plank or sole plate on the sill or grade), with folding wedges between the post tops and the template; never the window frame.

The template must carry the full weight of the wet arch, and of any brick laid above it, until the mortar can. A window frame is not built to take masonry load and would bow or break. Posts on solid bearing hold the template rigid, and the wedges allow fine adjustment now and controlled lowering later.

Exam trap: Shimming the template off the window head because it is conveniently at the right height: the frame deflects under the arch's weight and the arch sags.

Standard reference: RSOS 2021 H-23.03.01P

10 pairs · 1 decoyChecked at the end