Tilesetter Flashcards
Online Red Seal Exam Preparation, built on official standardsCards from
Blocks
How many cards
Card order
Show
100 cards selectedof 100
Set 1
In progress32known14to review again54not marked
Set 2
Finished twice78known22to review again0not marked
Cards by block
In each set of 100- AOccupational skills12 cards
- BSubstrate preparation15 cards
- CLayouts21 cards
- DMaterial preparation14 cards
- EMaterial setting24 cards
- FFinishing14 cards
Recent sessions
All sessions in Progress- 78%Set 2 · 100 cards · 78 known
- 72%Set 2 · 100 cards · 72 known
What is on a card
A-1.02Block A · Application
A tile-cleaner SDS requires chemical splash goggles. A face shield is also required for the pouring operation. How should the two protectors be worn?
- Answer
- Wear the splash goggles beneath the face shield.
- Why
- The shield adds facial protection while the goggles provide the specified splash protection for the eyes.
- Exam trap
- The face shield alone does not replace the splash goggles specifically required by the SDS.
From the Tilesetter standard: NOA 2010 A-1.02.02
Cards from
Blocks
How many cards
Show
100 cards selectedof 100
Sources
Blocks
- AOccupational skills
- BSubstrate preparation
- CLayouts
- DMaterial preparation
- EMaterial setting
- FFinishing
A-1.02Block A · task 1 · sub-task 2
Flashcards for every tradeBrowse the 20 free cards and explanations
A tile-cleaner SDS requires chemical splash goggles. A face shield is also required for the pouring operation. How should the two protectors be worn?
Answer: Wear the splash goggles beneath the face shield.
The shield adds facial protection while the goggles provide the specified splash protection for the eyes.
Exam trap: The face shield alone does not replace the splash goggles specifically required by the SDS.
Standard reference: NOA 2010 A-1.02.02
One installer can set 6 m² of tile per day. A 30 m² job also requires one full day of substrate preparation before setting, with no overlap. How many working days should be allowed?
Answer: Six working days.
Setting takes 30 ÷ 6 = 5 days; the separate preceding preparation day makes six.
Exam trap: Five days counts setting alone and omits the required preceding preparation day.
Standard reference: NOA 2010 A-3.01.06
Broken tile fragments repeatedly lodge across the cleaning vacuum’s hose inlet. What cleanup step should precede further fine-dust extraction?
Answer: Collect and remove the large fragments using suitable handling tools and dust controls.
Fine-dust equipment cannot reliably collect pieces larger than its inlet. Removing coarse debris first clears the intended path for subsequent fine cleanup.
Exam trap: A stronger vacuum setting does not make oversized pieces pass through the inlet.
Standard reference: NOA 2010 B-4.02.03
A roller-bonded sheet membrane has a free outer edge. A roller pass pushes an air pocket ahead of it while the adhesive remains workable. How should rolling progress to release the air?
Answer: Roll from the bonded area toward the free edge to expel the trapped air.
Progressive contact toward an escape edge displaces air instead of enclosing it beneath the sheet; the workable adhesive allows the specified roller bond to be completed.
Exam trap: Rolling from the free edge inward can close the air’s escape path and trap the pocket beneath the membrane.
Standard reference: NOA 2010 B-5.02.03
A loose-laid acoustic sheet overlaps its neighbour and forms a raised ridge beneath the planned tile bed. This system uses taped butt joints. What must be corrected before setting?
Answer: Reposition or trim the sheets to form the specified flat butt joint, then tape it as directed.
An unintended overlap creates local build-up; the specified butt-joint detail provides a flat support surface and controlled seam.
Exam trap: Flattening the mortar above the overlap leaves the unintended sheet build-up beneath it.
Standard reference: NOA 2010 B-6.01.03
Why does a steel tape have a sliding end hook for measurements against inside faces and over outside edges?
Answer: To compensate for hook thickness and retain the tape’s zero reference.
An outside measurement pulls the hook out; an inside measurement pushes it in. Its designed movement compensates for the thickness between the two contact faces, preserving the zero reference in either use.
Exam trap: Treating all hook movement as damage ignores its designed thickness compensation; excess or damaged movement still needs checking.
Standard reference: NOA 2010 C-7.01.01
A checkerboard layout contains six rows of seven tiles. The near-left corner starts dark. What colour reaches the diagonally opposite, far-right corner?
Answer: Light.
A checkerboard changes colour at each row or column step. The far-right corner is 5 row steps plus 6 column steps away: 11 changes. An odd number of changes gives the opposite of the starting dark colour.
Exam trap: Assuming opposite corners always match ignores the odd total of row and column steps in this particular rectangle.
Standard reference: NOA 2010 C-7.02.02
Successive unfinished riser faces lie at stations 0 and 300 mm in the ascending direction. Their nosings project toward lower stations by 20 and 25 mm, respectively. What is the going between the finished nosing lines?
Answer: 295 mm.
The lower finished nosing is at 0 − 20 = −20 mm; the next is at 300 − 25 = 275 mm. Their horizontal going is 275 − (−20) = 295 mm. Unequal projections change the spacing between finished references.
Exam trap: Using the 300 mm unfinished face spacing ignores the 5 mm difference between the two nosing projections.
Standard reference: NOA 2010 C-7.04.03
A joint survey records an existing movement separation as two straight segments meeting at a corner. The approved finish joint must follow it. How should the corner be carried into the tile setting-out plan?
Answer: Plot both surveyed segments and their actual intersection in the finish-joint plan.
The approved finish separation must follow the existing joint’s actual trace, including its change of direction. Retaining both segments and their vertex prevents a simplified straight line from bridging part of the separation.
Exam trap: Straightening the two segments for a cleaner tile grid departs from the existing joint trace.
Standard reference: NOA 2010 C-8.01.02
A pallet has crushed lower cartons, while the opened upper carton contains sound tiles. No tile from the crushed cartons has been inspected. What inspection is needed before accepting the affected part of the delivery?
Answer: Inspect product from the crushed lower cartons before accepting that affected portion.
Packaging damage identifies an area needing product inspection. Sound tiles from the upper carton do not establish the condition of unexamined tiles in the crushed cartons. Target the affected area and record the actual product condition.
Exam trap: Using the sound upper carton to clear the whole pallet does not sample the visibly affected area.
Standard reference: NOA 2010 D-9.02.03
A uniform 20 mm stone edge must have a full bullnose shaped as a semicircle tangent to the upper and lower faces. What radius produces that specified cross-section?
Answer: 10 mm.
The specified semicircle is tangent to both faces across the full 20 mm thickness. Its diameter is therefore 20 mm, so radius = 20 ÷ 2 = 10 mm. Confirm the shaped section against the approved profile.
Exam trap: Using a 20 mm radius gives a 40 mm diameter, which cannot fit this full semicircular edge section.
Standard reference: NOA 2010 D-10.02.07
A mortar-bed recipe specifies four loosely filled, level sand measures per cement measure. A worker packs each sand measure firmly before striking it level. Which batching practice must change to preserve the prescribed ratio?
Answer: Use loosely filled, level sand measures as the recipe specifies.
Volume recipes depend on a consistent filling condition. Firm packing increases sand mass within the same measure. Matching the number of buckets while changing how they are filled does not preserve the prescribed sand quantity.
Exam trap: Keeping the bucket count unchanged while packing the sand substitutes a greater sand quantity into the recipe.
Standard reference: NOA 2010 D-11.02.03
Fresh mortar transfers fully to a wall tile, but the tile creeps downward. Mixing and applied thickness match the product instructions; suitability for this vertical tile has not been verified. What setting-material working property must be checked?
Answer: Check the mortar's slip/sag resistance and qualification for the actual vertical tile application.
Full wet transfer confirms contact, but not the support needed before a wall tile sets. Correct mixing and thickness do not establish vertical-use slip resistance; verify that working property and the actual tile application.
Exam trap: Assume full transfer prevents sliding. Contact and immediate resistance to downward slip are different requirements.
Standard reference: NOA 2010 E-12 K1; E-12 K7
Why must an adhesive used for a porous stone accessory be checked for staining as well as bond strength?
Answer: A strong adhesive can still stain the porous accessory, so appearance compatibility must also be verified.
Bond strength and staining are separate properties. Porous stone may show migrated components at or around the adhesive contact even when the attachment remains sound.
Exam trap: Choose any adhesive that holds. A successful bond test alone does not rule out staining.
Standard reference: NOA 2010 E-12.03.03; E-12 K9
What corrosion mechanism can attack aluminium trim when it is electrically connected to copper in a persistently wet location?
Answer: Galvanic corrosion of the less noble aluminium.
Dissimilar metals in electrical contact with a wet electrolyte form a galvanic couple. Aluminium is less noble than copper and can corrode preferentially; adjoining-material compatibility therefore matters.
Exam trap: Assume aluminium cannot corrode because it does not form red rust. Red rust is not the only corrosion mechanism.
Standard reference: NOA 2010 E-12.05.03
Why must a slab-setting adhesive's permitted cured thickness be considered when choosing the bonding method?
Answer: The required layer must stay within the adhesive's thickness limits for the intended cured performance.
A bonding material is qualified for a specified layer geometry. A suitable thin bonding layer is not automatically a levelling filler for larger gaps, so the needed thickness affects method selection.
Exam trap: Use extra adhesive to bridge any gap. More thickness is not automatically within the product's qualified application.
Standard reference: NOA 2010 E-13.02.03; E-13 K4
A terrazzo primer permits topping only after it is tack-free and within 6 hours at 20°C. At 20°C it is tack-free after 3 hours; preparation checks pass. A helper wants to re-wet it because cement slurry must stay wet. What follows this primer's instructions?
Answer: Place the topping without re-wetting: this primer is tack-free and within its 6-hour window.
Bond-coat instructions are system-specific. At 20°C the primer meets its tack-free requirement after 3 hours and remains inside the 6-hour window; a wet cement-slurry rule does not apply to it.
Exam trap: Re-wet it by copying cement-slurry practice. This primer's accepted overcoat condition is tack-free, not re-wetted.
Standard reference: NOA 2010 E-14.02.02; E-14.02.05
A cured epoxy-grout film remains on ceramic tile after a compatible cement-haze cleaner leaves it unchanged. The tile surface passes the cleaner trial. What residue-specific cleaner class should be evaluated next?
Answer: Evaluate a manufacturer-approved epoxy-grout film/haze remover compatible with this tile.
Cured epoxy residue calls for a cleaner qualified for that resin film as well as the actual ceramic surface. An ineffective cement-haze cleaner should not simply be made stronger; evaluate the residue-specific class and follow its tested method.
Exam trap: Use a stronger cement-haze cleaner. Its intended residue differs from the cured epoxy film that remains.
Standard reference: NOA 2010 F-15.01.07; F-15 K9
A treatment is approved for cement grout but excluded from the glazed tile faces. The joints are narrow and clean. Which application approach keeps the treatment on its intended surface?
Answer: Use a narrow joint-directed applicator or brush and keep the treatment off the glazed faces.
Application tools must target the approved surface. A joint-directed tool treats the cement grout without spreading product onto tile faces excluded by this treatment.
Exam trap: Roll over the whole tile field. That puts treatment on an excluded finish as well as the grout.
Standard reference: NOA 2010 F-15.03.01; F-15.03.04
A terrazzo pocket repaired with colour-matched binder alone is sound but appears as a large plain patch in a chip-rich field. The repair must match that field's appearance. What component is missing from the repair mixture?
Answer: Matching aggregate chips are missing from the binder-only repair.
Repair soundness and binder colour already pass. The large plain patch lacks the field's exposed chips; a repair matching the field must restore that missing aggregate component through an approved method.
Exam trap: Add more binder pigment. Colour alone cannot reproduce the missing aggregate pattern.
Standard reference: NOA 2010 F-16.02.02